http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0559104-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_424db9d56b06a23aed410fcf5df652f3 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-004 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-00 |
filingDate | 1991-09-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c8b52d6a29c242343ab9e41120b9803d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1c158794864af384f8d1070d27742442 |
publicationDate | 1993-03-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0559104-A |
titleOfInvention | Inhibitor, polymerizer and prevention method for preventing adhesion of polymer scale |
abstract | (57) [Summary] [Structure] (A) An ethylenic double bond containing an aromatic amine compound, (B) an aromatic nitro compound, and (C) a condensation product of an aromatic hydroxy compound. A polymer scale adhesion preventive agent for polymerizing a monomer, a polymerization vessel in which a coating film comprising the inhibitor is formed, and a polymerization scale adhesion prevention method in which the polymerization is carried out in the polymerization vessel. [Effect] Adhesion of polymer scale can be effectively prevented. The resulting polymer has significantly less fish eye after molding and less deterioration of the initial colorability of the polymer after molding. |