http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0539385-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d5d04736b0b882a4f5a1e0e0e4cd8cbb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F291-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-26 |
filingDate | 1991-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5058239dada07af88ffd94dcf7425731 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f95e6c1f169de48bee10a3acfc1b794 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bda2f754f5212a2e2fd4f4aba5c5d4e6 |
publicationDate | 1993-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0539385-A |
titleOfInvention | Modified thermoplastic elastomer composition having good coatability and method for producing the same |
abstract | (57) [Summary] [Structure] 1) (A) Crystalline polyolefin resin, olefin polymer rubber, and unsaturated hydroxy compound are kneaded together with an organic peroxide to crosslink the olefin polymer rubber and unsaturated hydroxy. Modified thermoplastic elastomer composition comprising a modified thermoplastic elastomer obtained by simultaneously performing a graft reaction of a compound and (B) a hydroxyl group-containing polyolefin resin, and a method for producing the same 2) Thermoplastic obtained by kneading a hydroxyl group-containing polyolefin resin, an olefin polymer rubber, and an unsaturated hydroxy compound together with an organic peroxide, and then simultaneously crosslinking the olefin polymer rubber and grafting the unsaturated hydroxy compound. Elastomer composition and method for producing the same. [Effect] In the thermoplastic elastomer composition, urethane coating can be performed without a primer treatment, which has advantages such as cost reduction and number of steps. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-9817702-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0680743-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-4330356-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6297326-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5665820-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6107405-A |
priorityDate | 1991-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 99.