http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H05341571-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c391364e0741043fad9d4ca5347ce1a6 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate | 1992-06-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_814c21da849689dac9b95cf9ee181e28 |
publicationDate | 1993-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H05341571-A |
titleOfInvention | Method for manufacturing electrophotographic toner |
abstract | (57) [Summary] [Object] The present invention provides electrophotographic images of colored resin particles, which have excellent moisture resistance and fluidity, and have a particle size structure and a uniform particle size distribution suitable for use as a toner, in a resin polymerization step. It is an object of the present invention to provide a method for producing a toner for use. [Structure] A water-soluble polymer is used as a dispersion stabilizer during suspension polymerization of a monomer composition containing at least a polymerizable monomer, a colorant and a polymerization initiator, and the obtained polymer particles are By treating with a reducing agent, a toner having excellent moisture resistance can be manufactured. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008033304-A |
priorityDate | 1992-06-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 139.