Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6bfdf49224a405be1f7b653c56ebad94 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L93-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16F7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16F15-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L93-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L89-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-10 |
filingDate |
1992-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7887332548839f82a5de266e68887747 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_929705032e2047a544512102384aeb62 |
publicationDate |
1993-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H05339440-A |
titleOfInvention |
Polyolefin resin composition |
abstract |
(57) [Summary] [Structure] 5 to 70 parts by weight of rosin resin and 5 parts of polycarboxylic acid ester to 100 parts by weight of polyolefin resin. To 50 parts by weight, and a loss factor (tan δ) peak value of 0.1. Above, Young's modulus at the peak temperature is 5 × 10 8 Pa The above is the polyolefin resin composition characterized by the above, and a vibration energy absorbing material comprising the composition. [Effect] A vibration energy absorbing material having a high loss coefficient can be obtained. |