http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H05331267-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cff62ee19588f053fe1f229df4e6c756 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-18 |
filingDate | 1992-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1f78ade01b55691fce5d758d1c075469 |
publicationDate | 1993-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H05331267-A |
titleOfInvention | Wholly aromatic polyester |
abstract | (57) [Summary] [Purpose] To provide a novel wholly aromatic polyester having an excellent balance between molding processability and heat resistance. [Structure] The following structural units [I], [II] and [II] I] (provided that each structural unit is connected to each other by an ester bond), and a structural unit ([I] + [I I]) and the structural unit [III] are substantially equivalent, and the ratio [I] / [II] = 5/95 to 100 of the molar number of the structural unit [I] and the structural unit [II]. / 0, the wholly aromatic polyester having a melting temperature of 200 ° C. or higher, and the liquid crystalline wholly aromatic polyester having [I] / [II] = 5/95 to 45/55. [Chemical 1] (In the formula, Ar 1 and Ar 2 each independently have 6 to 18 carbon atoms. Is an aromatic hydrocarbon group) |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007254663-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115667359-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021241269-A1 |
priorityDate | 1992-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 139.