http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H05310967-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b27deaf45890893586c2ed77ac13dc32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9db45cbaec0651cacea17f30f366beee |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L73-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B11-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B15-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-24 |
filingDate | 1992-05-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4273e06de16fb14c9a28e56fe6d3237c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e70e9aaa2b900b099f050393e32e9afa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e4816a80b246c59d138a0253a1bbc7b1 |
publicationDate | 1993-11-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H05310967-A |
titleOfInvention | Method for producing thermosetting resin prepreg |
abstract | (57) [Summary] [Structure] Condensed polycyclic aromatic resin (eg, obtained by condensing naphthalene or a mixture of naphthalene and phenol with p-xylylene glycol in the presence of a reactive or water-insoluble acid catalyst). Resin) is dissolved in a mixed solvent of two or more kinds of organic solvents having different boiling points, the reinforcing fiber is impregnated with this solution, and then the solvent is removed to produce a thermosetting resin prepreg. It is preferable to use a mixed solvent of a solvent having a boiling point of 80 ° C. or less and a solvent having a boiling point of 100 ° C. or more, and desolvate at 80 ° C. or less so that 1 to 15% by weight of the solvent remains. [Effect] A prepreg having excellent heat resistance, mechanical properties, and moldability, and having appropriate drapeability and tackiness and good workability can be manufactured at a relatively low cost. Even if the reinforcing fibers are cloth, the resin can be sufficiently impregnated. |
priorityDate | 1992-05-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |