http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H05303918-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b0120933550ea729b9f3186c3772531b |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B7-08 |
filingDate | 1992-04-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7bb04472fc3c5e046c1677a92af7153b |
publicationDate | 1993-11-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H05303918-A |
titleOfInvention | Tape wire manufacturing method |
abstract | (57) [Summary] [Purpose] To provide a method of manufacturing a tape electric wire which has good flame retardancy and heat resistance and in which peeling of the conductor and the insulating layer does not occur even when subjected to the action of repeated bending. According to this production method, one side of the polyester film 1 is directly or through a cross-linking primer layer, and 10 to 90% by weight of a binary copolymer composed of styrene and ethylene-butylene or ethylene-propylene and partially cross-linked. Film A formed by forming an adhesive film layer 2 made of an adhesive composition containing 10 to 90% by weight of an olefinic thermoplastic elastomer in a free state or an uncrosslinked state as an essential component The step of forming the two adhesive film layers by arranging the surfaces of the two laminated films A, A on the side of the adhesive film layer facing each other, arranging a plurality of conductors 4 between the both surfaces, and then thermocompressing the whole. Embedding the conductor 4 with the adhesive film layer by integrating 2, 2; and irradiating the laminated film with a free reflection line or visible light to perform a crosslinking treatment on the integrated adhesive film layer. Process; |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8377515-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8377514-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9861941-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4712634-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007106982-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007012444-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011034703-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8263713-B2 |
priorityDate | 1992-04-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 43.