http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H05302063-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_05aa45bbbe92b502cb5976eadae82e24
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-4496
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-44
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-8061
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-7664
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-04
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-80
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-44
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-76
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-04
filingDate 1992-10-08-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a2f67ceb45ac5a46ad20be6ced676502
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e1eba24770cf771d3d03872af2a44eb8
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7c92f28fb3f6e354c170481878138398
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_555dabe910066fee4099e169c7683126
publicationDate 1993-11-16-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-H05302063-A
titleOfInvention Thermosetting coating for cathodic electrophoretic lacquer coating
abstract (57) [Summary] [Purpose] It contains a large amount of aromatic constituents in order to provide good corrosion resistance, and does not cause yellowing of white lacquer coating despite the presence of this aromatic constituent, It shows high reactivity by deblocking at a low baking temperature, forms a stable lacquer coating or electrophoretic coating bath despite the low deblocking temperature, and effectively prevents gelation and precipitation, and thus has no tendency to crystallize. It is an object of the invention to provide a crosslinking agent for cathodic electrophoretic lacquer coating which is not shown and can be produced easily and economically from raw materials which are economically and inexpensively available. (A) 50 to 95% by weight of a functionalized polymerization, polycondensation or polyaddition product and (B) 50 To 5% by weight of a blocked polymethylene polyphenyl isocyanate as a cross-linking agent, the cross-linking agent having the formula: And a block polyisocyanate mixture represented by the following formula, wherein n is a number from 0 to 10, wherein n in the formula is 0. A coating agent containing diphenylmethane diisocyanate in an amount of less than 25%.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-1073135-C
priorityDate 1991-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID82312
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID87058067
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID226405806
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID226405804

Total number of triples: 27.