http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H05295070-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2ba60be3b3f99c87e117c7f7c20b7071 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-685 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-60 |
filingDate | 1992-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_09256bb8a030d3aa059285aeee92fa15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ae680ad7736849d217b4783d3e4630b7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e77550b734a7f41162bc4300e9a16047 |
publicationDate | 1993-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H05295070-A |
titleOfInvention | Method for producing high molecular weight aliphatic polyester |
abstract | (57) [Summary] [Structure] [I] (1) Component of aliphatic dicarboxylic acid (or acid anhydride thereof) containing succinic anhydride as an essential component, (2) Polyhydric alcohol component, (3) Polyhydric component Obtained by polycondensation of 3 components of oxycarboxylic acid component, melting point 60 ° C. Above, polyester (a) 1 with number average molecular weight of 10,000 or more [II] 0.3 to 5 parts by weight of a polyvalent isocyanate is added to 00 parts by weight of the polyester (a) in a molten state at a melting point of 20,000 or more. [Effect] A method for producing a high molecular weight aliphatic polyester useful for various uses such as a film, a molded article, and a fiber is provided. |