http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H05287163-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-02 |
filingDate | 1992-04-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e778a725c933d66f5af8350a1696a822 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ba1d839d6b0a5ae3c86528debb889f62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0f2e6b67015260144231de9be2fc8569 |
publicationDate | 1993-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H05287163-A |
titleOfInvention | Thermoplastic resin composition |
abstract | (57) [Summary] [Structure] An aromatic vinyl monomer and a polar functional group-containing vinyl monomer, particularly an epoxy group-containing vinyl monomer or a carboxyl group-containing vinyl monomer, are added to a molten propylene polymer. A thermoplastic resin composition comprising a modified polypropylene obtained by a melt-kneading polymerization reaction in combination and a polyamide resin. [Effect] The composition of the present invention is excellent in mechanical strength and moldability, is superior to polyamide resin in non-water absorption and impact strength, and is superior to polypropylene in thermal deformability and flexural modulus. Provided is a thermoplastic molding material which is useful as a material and has well-balanced physical properties. It is extremely useful in the plastic molding field. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-9852199-A1 |
priorityDate | 1992-04-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 70.