Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2383-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-62 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J11-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-32 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-16 |
filingDate |
1992-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
1993-10-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H05271416-A |
titleOfInvention |
Pyrolysis method of silicone rubber vulcanizates |
abstract |
(57) [Summary] [Purpose] Silicone rubber vulcanizate pyrolysis method. [Structure] A method for thermally decomposing a silicone rubber vulcanizate, in which a vulcanizate is heated to 350 to 700 ° C. and volatile siloxane generated is condensed. EFFECTS Reusable products, in particular volatile siloxanes and fillers, are obtained. |