http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0525391-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L81-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L81-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-523 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-52 |
filingDate | 1991-07-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d27e1c2a0609ef207c35c8854e80ff85 |
publicationDate | 1993-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0525391-A |
titleOfInvention | Resin composition |
abstract | (57) [Summary] [Structure] A polymer alloy of PAS resin (A) and PPE resin (B) is mixed with phenyl resorcin. Aromatic polyphosphate compound (C) such as polyphosphate is added in an amount of 0.1 to 10 parts by weight based on 100 parts by weight of (A) + (B). [Effect] It has excellent heat resistance, flame retardancy, mechanical properties, and dimensional stability, as well as a good appearance due to improved compatibility. |