http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0525270-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2786295e61d306bf527292c8aea9ff7a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G69-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G81-00 |
filingDate | 1991-07-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d42b35c1ef227097770eefd651d7516 |
publicationDate | 1993-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0525270-A |
titleOfInvention | Polyamide-polyoxyethylene block copolymer containing phenolic hydroxyl group and method for producing the same |
abstract | (57) [Abstract] [Purpose] An object of the present invention is to provide an elastomer having heat resistance and conductivity which is useful as a polymer modifier and a polymer compatibilizer. A polycondensation product of a polyoxyethylene having a carboxyl group at both terminals and a polyamide having an aminoaryl group at both terminals, comprising a block unit (A) represented by the following general formula (I): A polyamide-polyoxyethylene block copolymer having a phenolic hydroxyl group, which comprises a block unit (B) represented by the general formula (II), and a method for producing the same. [Chemical 1] [Chemical 2] (In the formula, an integer of m = 1 to 300, an integer of n = 0 to 400, an integer of l = 1 to 400, l / (l + n) = 0.01 To 1, q is an integer of 1 to 40, Ar 1 is the following general formula (III). A divalent aromatic group having a structure represented by, Ar 2 is a divalent aromatic group containing a phenolic hydroxyl group, and R is a divalent organic group) |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002129101-A |
priorityDate | 1991-07-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 138.