Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6572309f22e2ad56c1390a78ac237bed |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K27-06 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-305 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-06 |
filingDate |
1992-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ca3ed6eef47760d42f24dd0367805c63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4c54b9a2251e11917a59fa44758fd8a0 |
publicationDate |
1993-09-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H05237909-A |
titleOfInvention |
Stretch film manufacturing method |
abstract |
(57) [Summary] (Corrected) [Objective] The present invention is a package that can shorten the manufacturing process without leaving or aging the molded film and can stably provide a stretch film for packaging excellent in packaging suitability. Provided is a method for manufacturing a stretch film. [Structure] The vinyl chloride resin composition is heated to a temperature of 25 to 35. A method for producing a stretch film for packaging, which comprises extruding a film extruded under an atmospheric condition of ° C and a relative humidity of 35 to 45% and winding the extruded film. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0788973-A |
priorityDate |
1992-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |