http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H05230713-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 |
filingDate | 1992-02-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cc9830f6a01ffbeab4a624cf22613d26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1853d30cbe9b17d9eea5115db338f55f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_68b62ac057a6197af3c35b0d8540c50e |
publicationDate | 1993-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H05230713-A |
titleOfInvention | Method for making easily dyeable polyester fiber |
abstract | (57) [Summary] [Purpose] It is possible to dye dark colors by atmospheric pressure dyeing. And to provide a method for producing easily dyeable polyester fiber which is excellent in process stability during spinning. [Structure] When melt-spinning a polyester in which 0.5 to 2.5 mol% of a phosphonium sulfonate represented by the following general formula is copolymerized at a take-up speed of 3500 to 8000 m / min, the draft ratio is 700 / M or more. (However, M represents the copolymerization amount (mol%) of the phosphonium sulfonate salt). |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008223148-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6652964-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012057291-A |
priorityDate | 1992-02-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 43.