http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H05214229-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-42 |
filingDate | 1992-02-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fd9daa5fb7c9bb23125f1fd142840933 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1f753734a81279883be563080414850e |
publicationDate | 1993-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H05214229-A |
titleOfInvention | Antistatic polyester composition |
abstract | (57) [Summary] [Purpose] To provide an antistatic polyester composition which has a good rudder biting property during molding and good melt molding stability. [Structure] 100 parts by weight of aromatic polyester, When (a) 0.2 to 30 parts by weight of a polyoxyalkylene polyether and (b) 0.05 to 10 parts by weight of an organic ionic compound are blended as an antistatic agent, the particle size of the dispersed antistatic agent is The product of the number of 2.5 μm or more and the compounding amount is 0. It is 1 or more and 1.0 or less. [Effect] A decrease in friction resistance between chips due to an antistatic agent is reduced, and stable melt molding can be performed. |
priorityDate | 1992-02-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |