Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be92719b856db86c092cc233e9512ca2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_758994071efb42b565fc2c04637be131 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-12 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M6-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 |
filingDate |
1991-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a04962cf3ce54c98fb2db5f7267d3e29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0eb3dbf5cde6a45e71a52db1406f8213 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9d011c4943dc6db32ad84b4a56051657 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_83255c5d6a596ee3a3199482ac0acbb8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_028dda8f74f08076d64bd77b70af53d7 |
publicationDate |
1993-08-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H05205515-A |
titleOfInvention |
Solid electrolyte, electrochemical device including the same, and method for forming solid electrolyte |
abstract |
(57) [Summary] [Object] To provide a solid electrolyte excellent in ionic conductivity and mechanical strength, an electrochemical device including the solid electrolyte, and a method for forming the solid electrolyte. A viscoelastic body containing a nonaqueous electrolytic solution in a high molecular weight polymer, the content of the nonaqueous electrolytic solution being 200% by weight or more based on the high molecular weight polymer, and the viscoelastic body Has an elastic modulus of 10 2 to 10 5 dyne / cm 2 and an elongation of 20. % Or more, and a solid electrolyte and an electrochemical device including the same. 100 parts by weight of unsaturated carboxylic acid ester is dissolved in the presence of a polymerization initiator in a non-aqueous electrolytic solution having an electrolyte salt concentration of 200 parts by weight or more of 1.0 mol / 1 or more to carry out a polymerization reaction, A method for forming a solid electrolyte, which comprises producing a polymer having viscoelasticity. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2013027767-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7105612-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002033129-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6096234-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004197069-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H10177814-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020523733-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-02080199-A1 |
priorityDate |
1990-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |