http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H05201800-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c62268de3e92657ca5b9adcac4778225 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C30B29-62 |
filingDate | 1992-01-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_af11496023db93d4b6255254ef3a56b1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dbf8ddfbdea81b9e7e2e8929c9c30368 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_79b9409cee3136b1c827cd4014ac295a |
publicationDate | 1993-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H05201800-A |
titleOfInvention | Method for manufacturing aluminum borate whiskers |
abstract | (57) [Summary] [Problem] To provide a method capable of producing aluminum borate whiskers having improved uniformity and having a uniform shape with high productivity, by using a basic aluminum salt aqueous solution. A method for producing aluminum borate whiskers, which comprises heat treating a mixture of a basic aluminum salt aqueous solution, a boron component-containing raw material, a melting agent and sulfuric acid. According to this manufacturing method, it is possible to manufacture aluminum borate whiskers having a uniform shape. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017031016-A |
priorityDate | 1992-01-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 39.