Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_847a4fdc318c1b72bd5bc8ba0f1f4680 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M6-164 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0569 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0568 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M6-16 |
filingDate |
1992-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d1db930ea4725f863536d781d8c2f568 |
publicationDate |
1993-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H05198315-A |
titleOfInvention |
Non-aqueous electrolyte |
abstract |
(57) [Summary] [Object] To provide an electrolyte solution for an electrochemical cell which can be stored at a high temperature for a long time without increasing the impedance of the cell to a level that substantially reduces the performance of the cell. [Structure] A mixture of a dioxolane-based solvent and an acyclic ether is used, and the weight ratio of the former to the latter is 1:99 to 45: 55, which is characterized in that the solute was dissolved in a mixture in which the volume ratio of the former and the latter was smaller than 40:60. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4668540-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005129481-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009021183-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008511962-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012514839-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005529467-A |
priorityDate |
1991-08-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |