http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0517571-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_95585944cd76ddfb6dc33ed2a0b84403 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G65-40 |
filingDate | 1991-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_34e7a372ced343bd5aa3f588b08d361e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_61b0ec14d0d45d4d7d961febfbef2a15 |
publicationDate | 1993-01-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0517571-A |
titleOfInvention | Polyether copolymer and method for producing the same |
abstract | (57) [Summary] [Object] To provide a polymer having excellent heat resistance, a high glass transition temperature, and a low hygroscopic property. [Structure] General formula [In the formula, Ar is (Y represents a divalent group having 1 to 13 carbon atoms). ] It consists of the repeating unit represented by these, and is 0.2g / which uses p-chlorophenol as a solvent. A polyether copolymer having a reduced viscosity of 0.3 dl / g or more measured at 60 ° C. in a dl-concentrated solution. |
priorityDate | 1991-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |