http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H05173273-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-015 |
filingDate | 1991-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a6b5b01afa9eb17fe07e3eb4f8b67b4c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7c9d11c306cd43969156b477b5c507e2 |
publicationDate | 1993-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H05173273-A |
titleOfInvention | Silver halide photographic light-sensitive material |
abstract | (57) [Summary] [Object] To provide a silver halide photographic light-sensitive material having high photographic sensitivity, small deterioration in sensitivity due to storage, and improved reciprocity law failure. A silver halide photographic light-sensitive material having at least one silver halide emulsion layer on a support, wherein the emulsion layer has a normal multi-layer structure of three or more layers having different silver iodide contents. Crystal grains are included, the silver iodide content of the outermost surface layer of the normal crystal grains is 6 mol% or less, the thickness is 0.025 μm or less, and the first inner layer is provided adjacent to the outermost layer. In the shell, the silver iodide content is higher than the silver iodide content of the outermost surface layer by 30 mol% or more, and the ratio of the first inner shell to the whole grains is 10% or less by volume. To do. |