Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1af8df51ce24ca931ae718fb747f6aa0 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B33-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B33-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B33-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-00 |
filingDate |
1991-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b9b8acc90d8643ef5094c13485ad56b9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_66286cb1b8e934fa4a1bc814e07b62fb |
publicationDate |
1993-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H05144570-A |
titleOfInvention |
Electroluminescent device |
abstract |
(57) [Abstract] [Purpose] To obtain an electroluminescent device with higher brightness. [Structure] In an electroluminescent device using a diamond crystal formed by vapor phase synthesis as a light emitting layer 4, the crystal defect density of the diamond crystal is set to 10 8 defects / cm 2 or less. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6819041-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1127936-A3 |
priorityDate |
1991-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |