http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H05127284-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-047 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-26 |
filingDate | 1991-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_55569e6008d4e67e405324f00d6cc9bb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0a1d1204b5a9b9ccdcd405da0482ae44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c4afff68f629ac062fd4c130171425f2 |
publicationDate | 1993-05-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H05127284-A |
titleOfInvention | Silver halide photographic light-sensitive material |
abstract | (57) [Abstract] [Purpose] To provide a silver halide photographic material which is excellent in drying property in ultra-rapid development processing and has less roller marks and scratch blackening. [Structure] In the hydrophilic colloid layer on the silver halide emulsion layer side, a developing solution containing a water-soluble maleic acid copolymer and containing no hardening agent and a fixing solution are used for a developing step of 8 seconds and a fixing step of 7. The silver halide photographic light-sensitive material is characterized in that the ratio of the swelling ratio at the completion of the water-washing process to the swelling ratio at the completion of the developing process is 1.0 or less when processed for 7 sec. |
priorityDate | 1991-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |