http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H05127282-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-815 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C11-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-04 |
filingDate | 1991-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b3bf20779ea662f1aaf3d3d002404a56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4aebf47064f4b4caf721a7b0c82975f4 |
publicationDate | 1993-05-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H05127282-A |
titleOfInvention | Silver halide photographic light-sensitive material |
abstract | (57) [Summary] [Purpose] To provide a silver halide photographic material which has good drying property in rapid development processing, small curl and excellent transportability. [Structure] The swelling rate of the total hydrophilic colloid layer on the side where the silver halide emulsion layer is present is 200% or less, the non-photosensitive hydrophilic colloid layer is on the opposite side, and the hydrophobic polymer layer is on the outside. And a non-photosensitive hydrophilic colloid layer and the hydrophobic polymer layer having substantially no swelling during processing. |