Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cebc9740ef706cde29e885504f274ffa |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K33-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-16 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C70-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-02 |
filingDate |
1991-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e06f05e31a766495ac9c0841edf66828 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_90debbf4462b8316ff48c9ba66138ea5 |
publicationDate |
1993-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H05125221-A |
titleOfInvention |
Resin composition having latent surface matting ability and molded article obtained from the resin |
abstract |
(57) [Summary] [Structure] The thermoplastic resin (A) has an average particle size of 1 μm. m or more and less than 10 μm, the absolute value of the difference in refractive index from the resin (A) is 0.01 or less, and 1 to 10% by weight of spherical glass beads (B) which are incompatible with the resin (a) are dispersed. A resin composition comprising: [Effect] A molded article having a sufficiently matt surface can also be obtained by heat stretch molding with a considerably low stretch ratio of slightly over 10%. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1249339-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6410147-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008248089-A |
priorityDate |
1991-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |