abstract |
(57) [Abstract] [Purpose] To obtain a rubber-modified thermoplastic resin composition having permanent antistatic property and free from delamination of resin after molding. [Structure] (A) 1 to 39% by weight of alkylene oxide polymer, (B) 10 to 99% by weight of rubber graft copolymer, Antistatic thermoplastic consisting of (C) 0 to 60% by weight of vinyl copolymer, 0.1 to 20% by weight of (D) modified vinyl copolymer and 0.01 to 1% by weight of (E) ammonium salt. Resin composition. |