http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H04325912-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B5-84
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B5-73929
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B5-7356
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-66
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-23
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-73
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-735
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12
filingDate 1991-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b84d81bb4025bc0aa5820b3993cbfb77
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1e1f1b44b453472820c720f81f970037
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_238624252692207675fe90e1a6bb1411
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_248e2a351b7775c73e13eb086cd188df
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e25c42237ddb4eb957f1745ded79d09a
publicationDate 1992-11-16-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-H04325912-A
titleOfInvention Magnetic recording tape
abstract PURPOSE: To provide the improved magnetic recording tape and particularly the magnetic recording tape for VTR which execute long-term recording. n CONSTITUTION: The Young's modulus in the longitudinal direction of the magnetic recording tape is ≥650kg/mm 2 and the Young's modulus in the transverse direction thereof is the same as the Young's modulus in the longitudinal direction or larger than this modulus. The thermal shrinkage when treated for 30 minutes at 100°C in the transverse direction is in a 1.0 to 3.0% range and the surface roughness Ra is ≤0.005μm. This magnetic recording tape consists of a base consisting of a biaxially oriented polyethylene-2, 6-naphthalate film having ≤0.01% oligomer deposition when treated for 5 minutes in the air kept at 160°C, a thin magnetic metallix film formed on one surface of this base and a coated film consisting of an org. high polymer contg. a lubricant applied on the other surface of the base. n COPYRIGHT: (C)1992,JPO&Japio
priorityDate 1991-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H02202925-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID4398214
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419584295
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID226503090
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID21864063

Total number of triples: 26.