http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H04296357-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6bfdf49224a405be1f7b653c56ebad94 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L81-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-18 |
filingDate | 1991-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b38f8cf340e173f14b8eed24fc9cef69 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b0cb780587f15123cf4d591510f9d3d6 |
publicationDate | 1992-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H04296357-A |
titleOfInvention | Polyphenylene sulfide resin composition |
abstract | PURPOSE: To provide a polyphenylene sulfide resin composition having improved toughness without damaging the characteristics thereof. n CONSTITUTION: A resin composition comprises (A) 50-99.5wt.%, preferably 70-98wt.%, of polyphenylene sulfide resin, (B) 50-0.5wt.%, preferably 30-2wt.%, of an acrylate ester copolymer obtained by copolymerizing 50-94mol.% of an acrylate ester (e.g. methyl acrylate, ethyl acrylate) with 50-6mol.% of a compound of formula I and/or a compound of formula II (R is 1-18C hydrocarbon having an ethylenic unsaturated bond: X is 1,4-phenylene, group of formula III, 0) (e.g. glycidyl acrylate), the sum of the components A and B being 100 pts.wt., and (C) 0-20 pts.wt. of a fibrous reinforcing material and/or a particulate reinforcing material (e.g. glass fibers, mica). n COPYRIGHT: (C)1992,JPO&Japio |
priorityDate | 1991-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |