http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0388849-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2b86357fa6e8b130b3e17c7f8e56856f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3467 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3445 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3442 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3477 |
filingDate | 1989-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0f29bd8228582b32a4f70a372dc52f84 |
publicationDate | 1991-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0388849-A |
titleOfInvention | Production of dust-proof plastic molded article |
abstract | PURPOSE: To obtain a plastic molded article having excellent dustproof property by blending a thermoplastic resin with a specific imidazole compound and subjecting the blend to heat molding. n CONSTITUTION: An imidazole compound having long-chain alkyl group at second position and being a compound selected from among an 2-alkylimidazole expressed by formula I (R 2 is 5-21C alkyl; R 4 is H or lower alkyl), acid addition salt thereof and metal complex thereof or a compound expressed by formula II or compound expressed by formula III is blended with a thermoplastic resin at an amount of 0.01-5wt.%, preferably 0.1-3wt.%. n COPYRIGHT: (C)1991,JPO&Japio |