http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H03243342-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_669c01133740c5233f2c8738904ea3af |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B44C3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B25-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-02 |
filingDate | 1990-02-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9a8e718924cdf053cda77fc95fa5b6e1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9576c3c3e5123f3d37e8384c76c9a7b5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d7322eb90839988fefc04cc2e7795ca9 |
publicationDate | 1991-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H03243342-A |
titleOfInvention | Decorative sheet for molding |
abstract | PURPOSE: To use for printing of a plastic molding, and give soft and not sticky feelings and senses by providing a transparent or translucent elastomer layer on the base material sheet of plastic having an excellent moldability. n CONSTITUTION: A decorative sheet for molding is constituted such that a transparent or translucent layer is provided on the base material sheet of plastic with a good moldability. The base material sheet is preferable to be thermally bonded or adhered therewith in accordance with the material of the plastic molding for integrating it. Showing examples of appropriate plastic as a material of the base material sheet, they are vinyl polymer such as polyvinyl chloride and polyvinyldene chloride, polyolefine such as ABS resin, polystylene, acrylic resin, polypropylene, and cellulose conductor, polyamide, polyester, polyvinyl alcohol, polycarbonate, polyethylene naphthalate, and polyether ether ketone, or the like. It is preferred to be thermoplastic for elastomer and should be chosen in respective groups of vinyl chloride, urethane, olefine, stylene, and ester. n COPYRIGHT: (C)1991,JPO&Japio |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-2836088-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1336476-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0752598-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5411783-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H072215-U http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007301903-A |
priorityDate | 1990-02-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 29.