http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H03126512-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6900162c0a64e321929e285aef793d73 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L31-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K75-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B62D1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-10 |
filingDate | 1989-10-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d11648427b68f14add0c00e49e3d3a02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b65f36be6d8cb6567cc7b64991535c0a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c79067b5356e4868be2cdbb47b6499fe http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8aba3ac6588b99aad8ab2d5c16603825 |
publicationDate | 1991-05-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H03126512-A |
titleOfInvention | Manufacture for urethane foam product |
abstract | PURPOSE:To enable formation of a skin coating made of thick urethane with a few number of times of coating work and in a short time, by a method wherein a bath liquid type skin urethane coating is stuck to a cavity surface by performing coating work becoming a cycle with casting and discharge into the cavity at least one time and dried forcibly further. CONSTITUTION:A matter which is in a mold clamping state and provided with casting and discharge holes 3, 4 for a skin urethane coating is used as a foam mold 1. Coating work becoming a cycle with the casting and discharge of the skin urethane coating into a mold (cavity) is performed at least one time in succession under a state where a mold is made into a clamped state by setting up a steering wheel core metal 6 to the mold 1. In this instance, a thick coating (0.5-1mm) is stuck and formed to a cavity 2 surface in one time. Forced drying of the coating is performed in succession, curing of the skin coating is advanced to such an extent that casting of a foamed urethane material is not affected and skin coating 7 comprised of the skin urethane coating is formed on the cavity 2 surface. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/ES-2150342-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2006010321-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-112020004086-T5 |
priorityDate | 1989-10-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Predicate | Subject |
---|---|
isDiscussedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419480927 http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID5641 |
Total number of triples: 22.