http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0297518-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-181 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-185 |
filingDate | 1988-10-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2989e6f8415e932109f0c9d62ac79558 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c88d7e24d2d2ac14dbc351c1bf3f4f2d |
publicationDate | 1990-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0297518-A |
titleOfInvention | Copolyester for heat-resistant packaging material |
abstract | PURPOSE: To improve heat resistance, gas barrier property, transparency and mechanical strengths by using a specific compd. as a comonomer. n CONSTITUTION: By copolymerizing an acid component contg. at least 80mole% terephthalic acid, a glycol component contg. at least 80mole% ethylene glycol, and 3-20mole% (based on said acid component) compd. of the formula (wherein R 1 and R 2 are each H or 1-3C alkyl; R 3 is H, or 1-10C alkyl, aralkyl or aryl), a copolyester for heat-resistant packaging material with a glass transition temperature of 83-90°C and an intrinsic viscosity (in a mixed solvent of phenol/ tetrachloroethane in a wt. ratio of 60/40, 35°C) of 0.4-1.0 is produced. n COPYRIGHT: (C)1990,JPO&Japio |