http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0258537-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_630b360599ea5cf4b5bcbc0c6c0a3e2d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G69-44 |
filingDate | 1988-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_17a5f445f59e856ee6b6a6cf8b12ce86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ce65fc915f079bde1b91ed9c98f3d4a3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2895ad1803ab379489039b3e187f84b1 |
publicationDate | 1990-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0258537-A |
titleOfInvention | Aromatic polyester amide and production thereof |
abstract | PURPOSE: To obtain a polyester amide with a specified structure capable of production by a conventional equipment and having soldering heat resistance, high elastic modulus, high strength and high fluidity. n CONSTITUTION: An aromatic polyester amide mainly composed of 1-30mol% aromatic aminocarboxylic acid residue represented by formula I (R 1 is H or 1-6C hydrocarbon), 2-50mol% 2,6-naphthalenedicarboxylic acid residue of formula II, 3-50mol% aromatic diol residue expressed by formula III (R 2 is divalent aromatic group), 0-45mol% aromatic dicarboxylic acid residue of formula IV and 0-75mol% aromatic oxycarboxylic acid residue of formula V and having ≥10 poise melt viscosity at 320°C, 100sec -1 . n COPYRIGHT: (C)1990,JPO&Japio |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8859711-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012530793-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012070774-A3 |
priorityDate | 1988-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 20.