Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L101-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L71-123 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-00 |
filingDate |
1988-07-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_889ce73c778ba003d1267cf370d97ff9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_63c6d6ceb6a2f4138209f207a8b02193 |
publicationDate |
1990-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H0232143-A |
titleOfInvention |
Thermoplastic resin composition |
abstract |
PURPOSE: To obtain a composition providing molded articles having excellent impact strength, tensile strength and tensile elongation, having whole components blended in excellent compatibility, by blending a thermoplastic resin with an epoxy group-containing styrene-based resin and styrene-based resin not containing epoxy group. n CONSTITUTION: A thermoplastic resin composition comprising (A) 5-95 pts.wt. thermoplastic resin containing a polar group selected from carboxyl group and hydroxyl group at an end or side chain and having 150-300°C melting point, (B) 0.01-50 pts.wt. epoxy-group-containing styrene-based resin, (C) 0-90 pts.wt. styrene-based resin not containing epoxy group and (D) 0-90 pts.wt. thermoplastic resin having molecular compatibility with the component C in an amount to give 100 pts.wt. total amounts and ≥5 pts.wt. sum of components C and D wherein the amount of the reaction product prepared by reaction between the component A and the component B is ≥3wt.% based on total weight of the components A, B and D and the ratio B/A of number-average molecular weight of the component A and the component B constituting the reaction product is 0.6-10.0 and intrinsic viscosity of the component A is ≥0.5dl/g. n COPYRIGHT: (C)1990,JPO&Japio |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H04100809-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020084037-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020084036-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020111011-A1 |
priorityDate |
1988-07-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |