http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H02210022-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F8-14 |
filingDate | 1989-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b21bf8ab47930a969eea3bf2afdf380d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d25fb0db805cdb9a1c5184e63928a9ab http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_755bb14ab9cbe67adbc2bbf1ee673b8c |
publicationDate | 1990-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H02210022-A |
titleOfInvention | Modified polyester conjugate fiber |
abstract | PURPOSE: To provide the title conjugate fiber excellent in color tone, slimy feel, flexibility, frictional characteristics and mechanical properties, suitable for woolly textiles, having sheath domain with each specific constituents and sectional area ratio. n CONSTITUTION: A wax 6-30 in acid value is first prepared by blending (1) 50-95wt.% of a higher aliphatic monocarboxylic ester such as melissyl palmitate and (2) 5-50wt.% of a hydrocarbon such as decane. Pts.wt., satisfying the relationship (R is sectional area ratio for sheath domain; P is pts.wt. of the wax), of the wax is blended with 100 pts.wt. of a polyester made up mainly of ethylene terephthalate and spun as the sheath domain so as to be 4-30% in the sectional area ratio for the sheath domain, thus obtaining the objective conjugate fiber. n COPYRIGHT: (C)1990,JPO&Japio |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008019528-A |
priorityDate | 1989-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 20.