http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H02198809-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_51ea8e921747f313703958e64d2aa3a7
classificationIPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K71-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L31-32
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-00
filingDate 1989-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4c9713f275f10f3215c5e18bedc05382
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_42bcd9f48545e4f78e75766fb7a3a964
publicationDate 1990-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-H02198809-A
titleOfInvention Preparation of semiconductive roll
abstract PURPOSE:To efficiently prepare a semiconductive roll having a stable electric resistance level by using a semiconductive polymer composition wherein a polymeric compound having an ether bond in the repeating unit thereof is used as a matrix and perchlorate is compounded with said matrix in a specific amount. CONSTITUTION:A semiconductive polymer composition wherein a polymeric compound having an ether bond in the repeating unit thereof is used as a matrix and perchlorate is contained in the matrix is used as a material for forming the semiconductive polymer layer 2 of a semiconductive roll. Perchlorate is compounded in an amount of 0.1 - 50pts.wt. per 100pts.wt. of the matrix component. Said polymer composition is prepared as a powdery mixture by sufficiently kneading perchlorate with the polymeric compound being the matrix component. A metal shaft body 1 is arranged to the recessed part 4 having a semicircular cross-section of a lower mold 6 and, after molds 5, 6 are clamped, the semiconductive polymer composition is injected in the molds 5, 6 under high pressure and this pressure is held for a predetermined time. The molds 5, 6 are cooled to solidify the polymer composition in the molds and the semiconductive roll is obtained. No perchlorate is exuded from the semiconductive polymer composition in the molds at the time of injection molding and the inner peripheral surface of the molds are not contaminated.
priorityDate 1989-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID123351
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID3283
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419485929
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559261

Total number of triples: 20.