http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H01167369-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6bfdf49224a405be1f7b653c56ebad94 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L87-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 |
filingDate | 1987-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cca7e207358b0eb1c9d70c03842695cc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_818f73b29c0d5df30ecf8790a2bd4c3f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a3922c3242277b9c82b52d54289db3fd |
publicationDate | 1989-07-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H01167369-A |
titleOfInvention | Weather resistance imparter for resin |
abstract | PURPOSE: To obtain a weather resistance imparter, consisting of triethylenediamine polymer, having a high thermal decomposition temperature, low volatility and excellent thermal stability in molding processing and suitable for polyolefin based resins. n CONSTITUTION: A weather resistance imparter consisting of triethylenediamine polymer having 1W50μm average particle diameter in an amount of 500W2000ppm is blended with a resin, especially polyolefin based resin. The above-mentioned polymer is preferably prepared by polymerizing triethylenediamine in the presence of sulfuric acid as a catalyst at a temperature within the range of 170W200°C. n COPYRIGHT: (C)1989,JPO&Japio |