http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H01149831-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-10 |
filingDate | 1987-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0e4c8bd62a660afcfd09ff59091786f9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c8855aea55a1144b4a75d542686cf11 |
publicationDate | 1989-06-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H01149831-A |
titleOfInvention | Thermoplastic aromatic polyimide polymer |
abstract | PURPOSE: To provide the title polyimide polymer having a specific inherent viscosity, excellent in the heat resistance and strength thereof and capable of being injection-molded, by comprising 3,3',4,4'-diphenyl sulfone tetracaboxylic acid dianhydride and a bis(aminophenoxy)benzene. n CONSTITUTION: (A) 3,3',4,4'-Diphenyl sulfone tetracarboxylic acid dianhydride and (B) an aromatic diamine having two connected diphenyl ether bonds [e.g., 1,4-bis(4-aminophenoxy)benzene] are mixed in a solvent to form a polyamic acid solution, which is added to a solution containing acetic anhydride, pyridine, etc., for a reaction thereof to provide the objective polymer containing the repeating units of the formula as a main component and having an inherent viscosity of 0.2W5.0dl/g measured under conditions consisting of a concentration of 0.5g/dl and a temperature of 30°C in concentrated sulfuric acid. n COPYRIGHT: (C)1989,JPO&Japio |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006282882-A |
priorityDate | 1987-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 26.