http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-6609727-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22F1-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C30-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22F1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C19-05 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C19-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C30-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22F1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C30-00 |
filingDate | 2019-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-6609727-B1 |
titleOfInvention | Alloy plate and manufacturing method thereof |
abstract | This alloy plate is, by mass, C: 0.0200% or less, Si: 0.02 to 2.00%, Mn: 0.02 to 2.00%, P: 0.050% or less, S: 0 0.0100% or less, Cr: 12.00 to 30.00%, Ni: 35.00 to 60.00%, N: 0.0200% or less, V: 0.02 to 1.00%, Nb: 2. More than 00%, 3.50% or less, Al: more than 2.60%, 4.00% or less, and optionally one of Ti, Mo, W, Cu, Co, B, Zr, Ca, Mg The balance is 10.00% or more of Fe, and the chemical composition is an impurity, the microstructure includes an austenite phase, the average crystal grain size of the austenite phase is 20 μm or more, and the austenite The average value of L1 / L2, which is the aspect ratio of the crystal grains of the phase, is 1.0 to 3.0 In the microstructure, no more than 15.0% is the area ratio of γ'-phase is 0.2% yield strength at room temperature 400MPa or more. |