http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-6083917-B1
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-144 |
filingDate | 2016-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-6083917-B1 |
titleOfInvention | Treatment agent for elastic fiber, elastic fiber, and method for producing polyurethane-based elastic fiber |
abstract | By promoting the release of N, N-dimethylacetamide used in the production of elastic fibers from elastic fibers, it is possible to prevent the occurrence of scum in the spinning process and processing process of elastic fibers and The processing agent for elastic fibers which improves property, the elastic fiber using such a processing agent, and the manufacturing method of a polyurethane-type elastic fiber are provided. An elastic fiber treatment agent containing a smoothing agent and a gelve alcohol having 12 to 24 carbon atoms is used. [Selection figure] None |
priorityDate | 2016-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links