titleOfInvention | Laminated film |
abstract | To provide a laminated film in which curling is suppressed and positioning of a mold during molding is easy. A laminated film in which at least a support and a resin layer formed of a resin are laminated, wherein the resin layer is measured by Raman spectroscopy in the MD direction, and the resin crystal part and the amorphous layer are measured. Part spectral intensity ratio A (crystal part / amorphous part) and spectral intensity ratio B (crystal part / amorphous part) of the resin part measured by Raman spectroscopy in the TD direction of the resin layer Part)) is an absolute value | B−A | of 0.00 to 0.60. [Selection figure] None |
priorityDate | 2014-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 111.