http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5799192-B1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-418 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2329-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2457-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2419-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-546 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-302 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-308 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-14 |
filingDate | 2015-02-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-5799192-B1 |
titleOfInvention | High adhesive resin composition, molded article and laminate comprising the same |
abstract | [PROBLEMS] To obtain a molded article and a laminate having flexibility, excellent mechanical properties, and excellent adhesion to a polar polymer, and stability after adhesion to an adherend. Provided are a molded article and a laminate. A polyvinyl acetal having a degree of acetalization of 50 to 85 mol%, a content of vinyl ester monomer units of 0.1 to 20 mol%, and a viscosity average polymerization degree of 200 to 5000, 230 ° C When the polyvinyl acetal heated for 3 hours is measured by gel permeation chromatography, the peak top molecular weight (A) measured by a differential refractive index detector and an absorptiometric detector (measurement wavelength 280 nm) are measured. The peak top molecular weight (B) is the following formula (1) (AB) / A <0.60 (1) And a polyvinyl acetal having an absorbance at a peak top molecular weight (B) of 0.50 × 10 −3 to 1.00 × 10 −2 ; polyester, polyamide, α-olefin (co) polymer, cellulose resin And a thermoplastic resin selected from acrylic resins and styrene resins. [Selection] Figure 1 |
priorityDate | 2014-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 408.