classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H19-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H19-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F236-04 |
filingDate | 2013-12-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2014-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-5632956-B1 |
titleOfInvention | Copolymer latex |
abstract | [Problem] To provide a copolymer latex capable of exhibiting sufficient adhesive strength, realizing a low viscosity, and having good operability during preparation of coated paper. A copolymer latex obtained by emulsion polymerization, wherein the copolymer comprises (a) 15 to 60% by mass of an aliphatic conjugated diene monomer, and (b) a single amount of an ethylenically unsaturated carboxylic acid. (C) 5 to 30% by mass of a vinyl cyanide monomer, and (d) 0 to 75% by mass of a monomer copolymerizable therewith. In the emulsion polymerization, by the time when the polymer conversion rate of the reaction system reaches 1.0%, the total amount of the (c) vinyl cyanide monomer is not charged, Copolymer which is produced by charging 80% by mass or more of the total amount of the above (c) vinyl cyanide monomer by 60% of the time until the end when the total amount of the monomer component has been charged. latex. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5870216-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2015012366-A1 |
priorityDate | 2013-07-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 165.