http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5358254-B2
Outgoing Links
Predicate | Object |
---|---|
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K25-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C61-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-40 |
filingDate | 2009-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2013-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-5358254-B2 |
titleOfInvention | Laminated body, stretched film, heat-shrinkable film, molded body, heat-shrinkable label, and container equipped with the label |
abstract | <P>PROBLEM TO BE SOLVED: To provide a laminate excellent in heat resistance and transparency, excellent in appearance, hardly peelable when treated even at high temperatures and high in inter-layer adhesiveness. <P>SOLUTION: The laminate includes a first layer composed of a resin composition based on a polyester type resin and a second layer composed of a resin composition based on a polystyrene type resin. Differences in storage modulus between the resin composition constituting the first layer and that constituting the second layer are ≤±2.0×10<SP>9</SP>Pa at 70°C, ≤±1.0×10<SP>9</SP>Pa at 80°C, ≤±7.0×10<SP>7</SP>Pa at 90°C and ≤±1.0×10<SP>7</SP>Pa at 100°C. <P>COPYRIGHT: (C)2011,JPO&INPIT |