http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5167681-B2
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-80 |
filingDate | 2007-04-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-03-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2013-03-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-5167681-B2 |
titleOfInvention | Method for producing nickel positive electrode for alkaline storage battery |
priorityDate | 2007-04-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 38.