http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5125054-B2
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-13 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B31-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C1-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-06 |
filingDate | 2006-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-01-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2013-01-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-5125054-B2 |
titleOfInvention | Powdered amorphous carbon and method for producing the same |
abstract | <P>PROBLEM TO BE SOLVED: To provide an amorphous carbon powder with high packing density, and an easy production method thereof. <P>SOLUTION: The amorphous carbon powder has packing density of 0.6-0.8 g/cm<SP>3</SP>. The production method of the amorphous carbon powder comprises a step of firing a compound of formula (1) (wherein R is a 1-12C hydrocarbon group optionally having a hydroxy group, an alkyl group, an alkoxy group, an aryl group, an aryloxy group, a sulfonyl group, a halogen atom, a nitro group, a thioalkyl group, a cyano group, a carboxy group, an amino group or an amide group; R' is a hydrogen atom or a methyl group; and n is 3, 5 or 7) in the presence of an oxidizing gas at ≤400°C and a step of carbonizing a fired product obtained in the previous step in an inert gas atmosphere. <P>COPYRIGHT: (C)2008,JPO&INPIT |
priorityDate | 2006-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 1257.