classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-00 |
filingDate | 2006-09-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2012-02-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2012-02-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-4869842-B2 |
titleOfInvention | Resin product manufacturing method and resin product repair method |
abstract | <P>PROBLEM TO BE SOLVED: To easily impart useful properties such as elasticity and repairability to a cured resin product while maintaining the strength at a certain extent. <P>SOLUTION: The resin product 40, 50 is produced by preparing a thermoplastic resin solution 20 by dissolving at least a thermoplastic resin 12 in a solvent 11 capable of dissolving the thermoplastic resin 12, preparing a mixed liquid 30 by mixing the thermoplastic resin solution 20 with a liquid thermosetting resin 21, and removing the solvent 11 from the mixed liquid 30. The resin product 50 can also be produced by preparing the thermoplastic resin solution 20 by dissolving at least the thermoplastic resin 12 in the solvent 11 without heating, preparing the mixed liquid 30 at least by mixing the thermoplastic resin solution 20 with the liquid thermosetting resin 21 and a curing agent 41, imparting a prescribed shape to the mixed liquid 30, and curing the thermosetting resin 21 at the same time as the removal of the solvent 11 by vaporization. <P>COPYRIGHT: (C)2008,JPO&INPIT |
priorityDate | 2006-09-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |