http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-3398404-B2
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2993 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G11B5-712 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G49-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01F1-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-712 |
filingDate | 1992-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2003-04-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2003-04-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-3398404-B2 |
titleOfInvention | Manufacturing method of magnetic particle powder for magnetic recording |