http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-3169581-U
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02A40-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02A10-26 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E02B3-043 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01K61-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01G33-00 |
filingDate | 2011-05-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2011-08-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2011-08-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-3169581-U |
titleOfInvention | Hardened product for seaweed formation |
abstract | The present invention provides a hardened product for creating seaweed beds that can efficiently supply divalent iron ions to living organisms. Cement, steel slag crushed to 40 mm or less, hardened hardwood chips of about 20 to 80 mm, and water are mixed, and the resulting mixture is poured into a mold. And it is made to cure in a mold until it hardens | cures. Next, the concrete obtained by curing in the mold is crushed so that the unit volume mass is 2 to 3 ton / m 3 , thereby obtaining the concrete for building a seaweed bed whose surface shape is a natural stone shape. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2014038596-A1 |
priorityDate | 2008-10-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 24.