http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2735936-B2
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C1-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C19-03 |
filingDate | 1990-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1998-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1998-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2735936-B2 |
titleOfInvention | Dispersion-strengthened Ni alloy powder excellent in sinterability and method for producing the same |
priorityDate | 1990-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links